Bubbles in epoxy: causes, prevention and fixes

Bubbles come from air whipped in while mixing, resin that's too cold or too thick, or air escaping from wood underneath. Which one you have decides the fix.

Where the bubbles come from

Almost every bubble in a pour has one of four sources. TotalBoat's TableTop instructions list all four:

  • Mixing. Stirring too fast, or with a drill mixer, whips air in. Thousands of tiny bubbles can make the batch look white, and the smaller they are, the harder it is for them to rise and pop.
  • Cold. Below about 60 °F (15 °C) resin is too thick to release air and level itself.
  • Too thick a coat. A coating epoxy poured past its maximum thickness (1/4 in, about 6 mm, for TableTop) holds on to its bubbles, even with a heat gun.
  • Unsealed wood. Air in the grain keeps rising into the curing epoxy. Heat makes this worse, not better.

Bubbles that keep appearing in one area long after the pour, often over knots, end grain or cracks, are almost always air from the wood, not from the mix.

Preventing bubbles

  • Work inside the product's temperature range (65–80 °F for TableTop) with the resin and hardener at room temperature.
  • Stir slowly by hand for the full mixing time, scraping the sides and bottom. Don't use a drill mixer for coating epoxy.
  • On wood, concrete and other porous surfaces, brush or spread a thin seal coat first (TotalBoat: about 1/16 in), let it cure hard, sand with 80–120 grit and wipe clean before the flood coat.
  • Never pour a coat thicker than the data sheet's maximum. For thick river or casting pours use a deep-pour epoxy and the deep pour planner to split the depth into layers.

Removing bubbles while the epoxy is wet

Let the pour sit for about 10 minutes so bubbles rise, then pass a heat gun or propane torch 6–8 in (15–20 cm) above the surface, moving constantly. Don't hold heat on one spot for more than a few seconds: it can scorch or yellow the surface, and it can push colorants around. Check again and repeat during the early cure (TotalBoat says the first 30 minutes). UltraClear warns never to heat its bar and table top epoxy more than 20 minutes after pouring.

Heat is for thin coating epoxy. Deep-pour products are designed to release air slowly on their own; follow your product's own instructions before torching one.

Fixing bubbles in cured epoxy

Once it has cured, heat won't help. Sand the bubbles out (UltraClear: wait at least 12 hours, start coarse and finish the whole surface at 220–320 grit), wipe the dust off with acetone or denatured alcohol, let it dry and pour a fresh flood coat. The sanded surface looks white, but the new coat makes it clear again. If you sand through to bare wood, seal it again first or the bubbles come back.

Work out how much epoxy the repair coat needs with the flood coat calculator, and split the batch into Part A and Part B with the mix ratio calculator.

Milky haze rather than distinct bubbles? See cloudy or yellow epoxy. Craters and pulled-back edges are fisheyes.

Plan a seal coat and flood coat

Epoxy bubble questions

Why does my epoxy keep getting bubbles after I torch it?

If new bubbles keep rising in the same spots, air is escaping from porous wood under the epoxy. TotalBoat says heat makes this worse. Let it cure, sand, apply a seal coat and pour the flood coat again.

Is a heat gun or a torch better for epoxy bubbles?

TotalBoat's instructions allow either, held 6–8 in above the surface and kept moving. A torch is an open flame, so keep it away from solvents and tape. Follow your own product's instructions.

How do I get bubbles out of cured epoxy?

Sand them out, clean off the dust with acetone or denatured alcohol, and pour a new flood coat. Heat does nothing once the epoxy has cured.

Does warming the resin reduce bubbles?

Cold resin is thick and traps air; TotalBoat lists below 60 °F as a cause of bubbles. Keep resin, hardener and the room inside the data sheet's temperature range.